LHC束流转储的尸检
Autopsy of an LHC Beam Dump

原始链接: https://home.cern/news/news/accelerators/autopsy-lhc-beam-dump

欧洲核子研究组织(CERN)对大型强子对撞机(LHC)的一个放射性束流吸收器进行了“尸检”,以了解氮泄漏的原因,并为未来的束流吸收器设计提供信息。经过十年的运行,吸收器出现了退化,内窥镜检查发现挤压石墨盘意外开裂。由于放射性,切割吸收器非常具有挑战性。CERN的团队开发了使用自动化圆锯和机械臂的远程切割技术。“尸检”证实挤压石墨盘破裂,而低密度和高密度石墨状况良好。这些发现证实了在运行3中使用低密度和高密度石墨的合理性,但也排除了在未来设计中使用挤压石墨。该结果将有助于在2023年前为LHC设计备用吸收器,并为高光度大型强子对撞机(HL-LHC)设计吸收器。尽管能量水平提高,但对当前吸收器的改进预计将提高其在运行3中的耐受性。

一个Hacker News帖子讨论了一篇关于CERN大型强子对撞机束流阻挡器尸检的文章。评论者分享了一些轶事,其中一人帮助组装了LHCb项目的探测器部件。几位用户评论了CERN内部与科幻游戏环境的相似之处。这引发了关于以CERN为背景的游戏的讨论,提到了《命运石之门》(其中虚构的CERN是反派)和《Robotics;Notes》。另一位评论者提到最近由于故障使用了束流阻挡器。最后,有人提出了一个关于束流阻挡器组件(特别是钢制外壳和石墨)的放射性以及发生的嬗变性质的问题。

原文

For the first time at CERN, an autopsy has been carried out on a radioactive beam dump. Inspection of the inner workings of the device helped the teams to find out more about how materials behave under the impact of high-energy beams

During LS2, the LHC’s two external beam dumps were removed from the tunnel and replaced with spare ones. After ten years of operation, they were showing signs of degradation, notably nitrogen leaks. Before being installed, the spare dumps were modified and upgraded to prevent the same problems from occurring during Run 3 (see this Bulletin article published in 2020).

To find out more about the cause of the nitrogen leaks, an endoscopy was carried out in July 2020. It revealed unexpected cracks in the beam dump’s two extruded graphite discs (see box). An action plan was drawn up by the SY-STI (Sources, Targets and Interactions) group as more information was needed with Run 3 on the horizon, especially with a view to designing new spare beam dumps for the LHC and, beyond that, beam dumps for the HL-LHC. To access the dump’s three main components – high-density, low-density and extruded graphite (see below) – there was only one possible solution: perform an “autopsy” on one of the dumps. Given its radioactivity levels, this was easier said than done.

“To reach the heart of the beam dump, we needed to be able to open it…,” says project leader Ana-Paula Bernardes. “But its duplex-stainless-steel-alloy housing was extremely difficult to cut. The first attempt, in January 2021, under a framework contract, was unsuccessful: it was impossible to cut through it manually without exceeding the radiation dose limits. We considered outsourcing the job to a specialised external company with the right equipment for the task, but the costs and time frames were incompatible with the project.”

home.cern
Top: Longitudinal test cut with the circular saw, performed by the SY-STI group. Solution chosen for the cutting of the radioactive dump. Middle: Positioning of the automated, rail-mounted circular saw for the first radial cut, performed by the SY-STI group. Bottom: The first longitudinal cut. (Images: CERN)

Thanks to the expertise and versatility of CERN’s teams, a solution was eventually found in house: the SY-STI and BE-CEM (Controls, Electronics and Mechatronics) groups worked together to develop two techniques that would allow the dump’s housing to be cut remotely. The first involved an automated circular saw mounted on a rail, and the second a robot arm equipped with a cutter.

home.cern,Accelerators
Longitudinal test cut with the robot arm, performed by the BE-CEM group. (Image: CERN)

Several trial runs were carried out on a mock-up in order to “choreograph” the operation and thus limit, as far as possible, the time spent in close proximity to the dump. The circular saw was ultimately used to make five cuts, in a radiation airlock installation created specially for the job: two radial cuts to separate the low-density graphite block and three longitudinal cuts to remove the stainless-steel-alloy housing.

home.cern,Accelerators
The highly radioactive stainless-steel-alloy housing is removed by the EN-HE (Handling Engineering) group to allow access to the low-density graphite.(Image: CERN)

“As the endoscopy had already shown, both extruded graphite discs were cracked. Against all expectations, the low-density graphite was generally in good condition, as were the high-density-graphite blocks,” says Ana-Paula Bernardes.

home.cern,Accelerators
The upstream extruded graphite disc (the first to be hit by the beam) is cracked. (Image: CERN)

“It was important to check the condition of the various components of the dump and establish how resistant they were, for various reasons,” explains Marco Calviani, leader of the Targets, Collimators and Dumps (STI-TCD) section in the SY department. “First of all, we needed to be sure that the dumps currently installed in the LHC – which are built from the same components as the autopsied dump – would withstand the energy levels of Run 3; next, we wanted to know what strategy to adopt for the two new spare dumps, which we need to design and manufacture by 2023, and especially for the dumps for the future HL-LHC.”

The results of the autopsy validated the use of low-density and high-density graphite for Run 3, but ruled out the use of extruded graphite for the design of the spare dumps. Other studies are under way at the HiRadMat facility (see the corresponding article entitled “What will the future LHC beam dumps be made of?”) to confirm these results and to test new materials, notably for the HL-LHC beam dumps. What about the dumps that are already in place? “The modifications made before their installation should greatly improve their resistance for Run 3, even though the energy to be dissipated is set to increase from 320 MJ to 540 MJ,” says Marco Calviani. “Don’t forget that the previous dumps withstood the onslaught for ten years!”


What are the current LHC beam dumps made of?

home.cern,Accelerators
(Image: CERN)

The LHC’s external beam dumps comprise a graphite dump measuring 8.5 metres in length and 722 mm in diameter, contained in a 12-mm-thick 318LN stainless-steel-alloy tube. In total, each dump weighs 6.2 tonnes.

Each beam dump is made of several graphite blocks of varying density: high-density isostatic graphite; a stack of 1700 2-mm-thick low-density expanded graphite discs; and two extruded graphite discs (the black bands), which hold the low-density graphite stack together.